Standard welding procedure specification (SWPS) for argon plus 25% carbon dioxide shielded flux cored arc welding of carbon steel (M-1/P-1/S-1, groups 1 and 2), 1/8 through 1-1/2 inch thick, E7XT-X, As-welded or PWHT condition, primarily pipe applications
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of carbon steel to austenitic stainless steel (M-1 to M-8, P-8, or S-8), 18 through 10 gage, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005881095 / 2003-01-06
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of carbon steel to austenitic stainless steel (M-1 to M-8, P-8, or S-8), 18 through 10 gage, in the as-welded condition, with or without backing : AWS B2.1-1/8-006:2002.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 1990, TX 2-839-083.
Copyright Note:
C.O. correspondence.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode
Copyright Claimant:
American Welding Society
Notes:
Supersedes ANSI/AWS B2.1.006-90.
Names:
American Welding Society (599 documents)
example document: Standard welding procedures specification (WPS) for gas tungsten arc welding followed by shielded metal art welding for austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, ER3XX, E3XX-XX as-welded condition, primarily pipe applications
example document: Standard welding procedures specification (WPS) for gas tungsten arc welding followed by shielded metal art welding for austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, ER3XX, E3XX-XX as-welded condition, primarily pipe applications
|
|
Specification for thermal spray equipment acceptance inspection
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005900828 / 2004-01-13
Date of Publication:
January 5, 2004
Date of Creation:
2004
Title:
Specification for thermal spray equipment acceptance inspection : AWS C2.21M/C2.21:2003, an American national standard.
Description:
19 p.
Variant title:
Specification for thermal spray equipment acceptance inspection : AWS C2.21M/C2.21:2003, an American national standard.
Copyright Claimant:
American Welding Society
Names:
Recommended practices for the welding of rails and related rail components for use by rail vehicles
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005925956 / 2004-02-06
Date of Publication:
February 2, 2004
Date of Creation:
2004
Title:
Recommended practices for the welding of rails and related rail components for use by rail vehicles.
Basis of Claim:
New Matter: new and rev. text, ill. and compilation.
Previous Registration:
Prev. reg. 1994, TX 3-957-037.
Series:
AWS D15.2:2003
Description:
37 p.
Number of similar titles:
1
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for copper and copper alloy gas welding rods
example document: Specification for copper and copper alloy gas welding rods
Specification for filler metals for brazing and braze welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005945051 / 2004-04-05
Date of Publication:
March 26, 2004
Date of Creation:
2004
Title:
Specification for filler metals for brazing and braze welding : AWS A5.8/A5.8M: 2004 : an American national standard.
Basis of Claim:
New Matter: new & rev. text, ill., & compilation of data.
Previous Registration:
Prev. reg. 1993, TX 3-510-198.
Imprint:
Miami : American Welding Society, 2004.
Description:
37 p.
Number of similar titles:
1
Variant title:
Specification for filler metals for brazing and braze welding : AWS A5.8/A5.8M: 2004
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Method for sound level measurement of manual arc welding and cutting processes
example document: Method for sound level measurement of manual arc welding and cutting processes
Specification for titanium and titanium-alloy welding electrodes and rods
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005947437 / 2004-03-22
Date of Publication:
March 12, 2004
Date of Creation:
2004
Title:
Specification for titanium and titanium-alloy welding electrodes and rods : AWS A5.16/A5.16M:2004 an American national standard.
Basis of Claim:
New Matter: additions, revisions, ill, & compilation of data.
Previous Registration:
Prev. reg. 1990, TX 2-847-582.
Imprint:
Miami : American Welding Society, c2004.
Description:
19 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Operator's manual for oxyfuel gas cutting
example document: Operator's manual for oxyfuel gas cutting
AWS D16.1M/D16.1:2004
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005975003 / 2004-04-30
Date of Publication:
April 23, 2004
Date of Creation:
2004
Title:
AWS D16.1M/D16.1:2004 : Specification for robotic arc welding safety.
Series:
15 p
Other Title:
Specification for robotic arc welding safety
15 p.
15 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Recommended practices for welding of chromium-molybdenum steel piping and tubing
example document: Recommended practices for welding of chromium-molybdenum steel piping and tubing
Specification for the qualification of welding fabricators
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005976792 / 2004-05-17
Date of Publication:
May 10, 2004
Date of Creation:
2004
Title:
Specification for the qualification of welding fabricators : AWS B5.17:2004 : an American national standard.
Basis of Claim:
New Matter: new & rev. text and compilation of data.
Previous Registration:
Prev. reg. 2001, TX 5-377-458.
Description:
8 p.
Number of similar titles:
1
Variant title:
Specification for the qualification of welding fabricators : AWS B5.17:2004
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for nickel and nickel alloy covered welding electrodes
example document: Specification for nickel and nickel alloy covered welding electrodes
Specification for the application of thermal spray coatings (metallizing) of aluminum, zinc, and their alloys and composites for the corrosion protection of steel
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006028434 / 2003-09-08
Date of Publication:
August 26, 2003
Date of Creation:
2003
Title:
Specification for the application of thermal spray coatings (metallizing) of aluminum, zinc, and their alloys and composites for the corrosion protection of steel.
Copyright Note:
C.O. correspondence.
Series:
AWS C2.23M/C2.23:2003 ; NACE no. 12, SSPC-CS 23.00
Description:
37 p.
Variant title:
Specification for the application of thermal spray coatings (metallizing) of aluminum, zinc, and their alloys
Other Title:
AWS C2.23M/C2.23:2003 ; NACE no. 12, SSPC-CS 23.00
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Standard welding procedures specification (WPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, E3XX-XX as-welded condition, primarily pipe applications
example document: Standard welding procedures specification (WPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, E3XX-XX as-welded condition, primarily pipe applications
Methods for sampling and analyzing gases from welding and allied processess
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006028435 / 2003-04-18
Date of Publication:
August 6, 2003
Date of Creation:
2003
Title:
Methods for sampling and analyzing gases from welding and allied processess.
Basis of Claim:
New Matter: new and rev. text, ill. and compilation.
Previous Registration:
Prev. reg. 1997, TX 4-523-872.
Copyright Note:
C.O. correspondence.
Series:
AWS F1.5M:2003
Description:
44 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Recommended practices for root pass welding of pipe without backing
example document: Recommended practices for root pass welding of pipe without backing
Guide for estimating welding emissions for EPA and ventilation permit reporting
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006028436 / 2003-04-11
Date of Publication:
August 7, 2003
Date of Creation:
2003
Title:
Guide for estimating welding emissions for EPA and ventilation permit reporting.
Copyright Note:
C.O. correspondence.
Series:
AWS F1.6:2003
Description:
8 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for carbon steel covered arc welding electrodes
example document: Specification for carbon steel covered arc welding electrodes
Specification for the qualification of welding inspectors
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006028437 / 2003-07-08
Date of Publication:
June 19, 2003
Date of Creation:
2003
Title:
Specification for the qualification of welding inspectors.
Copyright Note:
C.O. correspondence.
Series:
AWS B5.1:2003
Description:
12 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for carbon steel electrodes for flux cored arc welding
example document: Specification for carbon steel electrodes for flux cored arc welding
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert root of austenitic stainless steel
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006085663 / 2004-12-16
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert root of austenitic stainless steel : AWS B2.1-8-215:2001.
Basis of Claim:
New Matter: additions and revisions.
Previous Registration:
Prev. reg. 2000, TX 5-355-643.
Description:
1 v.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert root of austenitic st
Copyright Claimant:
American Welding Society
Names:
Recommended practices for automotive weld quality-resistance spot welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006119080 / 2005-02-10
Date of Publication:
January 28, 2005
Date of Creation:
2005
Title:
Recommended practices for automotive weld quality-resistance spot welding : AWS D8.7M:2005.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1988, TX 2-431-369.
Number of similar titles:
1
Variant title:
Recommended practices for automotive weld quality-resistance spot welding : AWS D8.7M:2005.
Copyright Claimant:
American Welding Society
Notes:
Cataloged from appl. only.
Names:
American Welding Society (599 documents)
example document: Specification for carbon steel electrodes for flux cored arc welding
example document: Specification for carbon steel electrodes for flux cored arc welding
Speficiation for zirconium and zirconium-alloy welding electrodes and rods
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006119081 / 2005-02-10
Date of Publication:
January 28, 2005
Date of Creation:
2005
Title:
Speficiation for zirconium and zirconium-alloy welding electrodes and rods : AWS A5.24/A5.24M:2005.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1990, TX 2-847-584.
Variant title:
Speficiation for zirconium and zirconium-alloy welding electrodes and rods : AWS A5.24/A5.24M:2005.
Copyright Claimant:
American Welding Society
Notes:
Cataloged from appl. only.
Names:
American Welding Society (599 documents)
example document: Recommended practices for welding austenitic chromium-nickel stainless steel piping and tubing
example document: Recommended practices for welding austenitic chromium-nickel stainless steel piping and tubing
Specification for carbon steel electrodes for flux cored arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006162287 / 2005-04-25
Date of Publication:
April 19, 2005
Date of Creation:
2005
Title:
Specification for carbon steel electrodes for flux cored arc welding : AWS A5.20/A5.20M:2005.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 1995, TX 4-172-759.
Number of similar titles:
2
Variant title:
Specification for carbon steel electrodes for flux cored arc welding : AWS A5.20/A5.20M:2005.
Copyright Claimant:
American Welding Society
Notes:
Cataloged from appl. only.
Names:
American Welding Society (599 documents)
example document: Recommended practices for gas metal arc welding
example document: Recommended practices for gas metal arc welding
Specification for the qualification of robotic arc welding personnel
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006165365 / 2005-03-25
Date of Publication:
March 23, 2005
Date of Creation:
2005
Title:
Specification for the qualification of robotic arc welding personnel : AWS D16.4M/D16.4:2005.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 2000, TX 5-183-489.
Number of similar titles:
1
Variant title:
Specification for the qualification of robotic arc welding personnel : AWS D16.4M/D16.4:2005
Copyright Claimant:
American Welding Society
Notes:
Cataloged from appl. only.
Names:
Specification for welding of rotating elements of equipment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006165366 / 2005-03-25
Date of Publication:
March 23, 2005
Date of Creation:
2005
Title:
Specification for welding of rotating elements of equipment : AWS D14.6M/D14.6M:2005.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 1996, TX 4-400-382.
Number of similar titles:
1
Variant title:
Specification for welding of rotating elements of equipment : AWS D14.6M/D14.6M:2005
Copyright Claimant:
American Welding Society
Notes:
Cataloged from appl. only.
Names:
American Welding Society (599 documents)
example document: Specification for carbon steel covered arc welding electrodes
example document: Specification for carbon steel covered arc welding electrodes
Specification for nickel and nickel-alloy bare welding electrodes and rods
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006183381 / 2005-05-16
Date of Publication:
May 4, 2005
Date of Creation:
2005
Title:
Specification for nickel and nickel-alloy bare welding electrodes and rods : AWS A5.14/A5.14M:2005.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 1998, TX 4-737-683.
Copyright Note:
Cataloged from appl. only.
Number of similar titles:
1
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Standard procedures for calibrating magnetic instruments to measure the Delta ferrite content of austenitic stainless steel weld metal
example document: Standard procedures for calibrating magnetic instruments to measure the Delta ferrite content of austenitic stainless steel weld metal
Specification for low-alloy steel electrodes and rods for gas shielded arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006188251 / 2005-06-22
Date of Publication:
June 10, 2005
Date of Creation:
2005
Title:
Specification for low-alloy steel electrodes and rods for gas shielded arc welding.
Basis of Claim:
New Matter: new and rev. text, ill. and compilation.
Previous Registration:
Prev. reg. 1996, TX 4-400-387.
Copyright Note:
Cataloged from appl. only.
Series:
AWS A25.2/A5.28M:2005
Number of similar titles:
1
Copyright Claimant:
American Welding Society
Names:
Specification for welding of industrial and mill cranes and other material handling equipment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006188252 / 2005-06-22
Date of Publication:
June 10, 2005
Date of Creation:
2005
Title:
Specification for welding of industrial and mill cranes and other material handling equipment.
Basis of Claim:
New Matter: new and rev. text., ill,, & compilation.
Previous Registration:
Prev. reg. 1998, TX 4-779-159.
Series:
AWS D14.1/D14.1M:2005
Number of similar titles:
1
Copyright Claimant:
American Welding Society
Names:
Guide for aluminum hull welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006201089 / 2004-03-15
Date of Publication:
March 12, 2004
Date of Creation:
2004
Title:
Guide for aluminum hull welding : AWS D3.7:2004.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 1990, TX 2-866-648.
Copyright Note:
C.O. correspondence.
Cataloged from appl. only.
Cataloged from appl. only.
Number of similar titles:
2
Other Title:
AWS D3.7:2004
Copyright Claimant:
American Welding Society
Names:
Safety in welding, cutting, and allied processes
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006212175 / 2005-08-23
Date of Publication:
August 16, 2005
Date of Creation:
2005
Title:
Safety in welding, cutting, and allied processes : ANSI Z49.1:2005.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 1999, TX 4-957-558.
Copyright Note:
Cataloged from appl. only.
Number of similar titles:
2
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for corrosion-resisting chromium and chromium-nickel steel covered welding electrodes
example document: Specification for corrosion-resisting chromium and chromium-nickel steel covered welding electrodes
Specification for the qualification of welder test facilities
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006220802 / 2005-04-11
Date of Publication:
April 8, 2005
Date of Creation:
2005
Title:
Specification for the qualification of welder test facilities : AWS B5.4:2005.
Copyright Note:
C.O. correspondence.
Cataloged from appl. only.
Cataloged from appl. only.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Laboratory method for measuring fume generation rates and total fume emission of welding and allied processes
example document: Laboratory method for measuring fume generation rates and total fume emission of welding and allied processes
Specification for the qualification of resistance welding technician
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006220803 / 2005-04-11
Date of Publication:
April 8, 2005
Date of Creation:
2005
Title:
Specification for the qualification of resistance welding technician : AWS C1.5:2005.
Copyright Note:
C.O. correspondence.
Cataloged from appl. only.
Cataloged from appl. only.
Copyright Claimant:
American Welding Society
Names:
AWS A5.11/A5.11M:2005, specification for nickel and nickel-alloy welding electrodes for shielded metal arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006232379 / 2005-09-12
Date of Publication:
September 2, 2005
Date of Creation:
2005
Title:
AWS A5.11/A5.11M:2005, specification for nickel and nickel-alloy welding electrodes for shielded metal arc welding.
Basis of Claim:
New Matter: compilation, revisions, additions.
Previous Registration:
Prev. reg. 1998, TX 4-776-968.
Copyright Note:
Cataloged from appl.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Commentary on structural welding code--aluminum
example document: Commentary on structural welding code--aluminum
AWS C3.8M/C3.8:2005, specification for the ultrasonic examination of brazed joints
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006235354 / 2005-09-19
Date of Publication:
September 7, 2005
Date of Creation:
2005
Title:
AWS C3.8M/C3.8:2005, specification for the ultrasonic examination of brazed joints.
Basis of Claim:
New Matter: compilation, revisions, additions.
Previous Registration:
Prev. reg. 1990, TX 2-866-696.
Copyright Note:
Cataloged from appl.
Copyright Claimant:
American Welding Society
Names:
AWS A5.29/A5.29M
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006235798 / 2005-09-14
Date of Publication:
September 6, 2005
Date of Creation:
2005
Title:
AWS A5.29/A5.29M : 2005, specification for low-alloy electrodes for flux cored arc welding.
Basis of Claim:
New Matter: revisions & additions, ill. & updating.
Previous Registration:
Prev. reg. 1998.
Copyright Note:
Cataloged from appl. only.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: The Metric system, welding terms and symbols
example document: The Metric system, welding terms and symbols
Specification for carbon steel electrodes and rods for gas shielded arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006236622 / 2005-09-21
Date of Publication:
September 14, 2005
Date of Creation:
2005
Title:
Specification for carbon steel electrodes and rods for gas shielded arc welding : AWS A5.18/A5.18M:2005.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2001, TX 5-393-063.
Copyright Note:
Cataloged from appl. only.
Number of similar titles:
1
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for low alloy steel filler metals for gas shielded arc welding
example document: Specification for low alloy steel filler metals for gas shielded arc welding
AWS D14.4/D14.4M:2005, specification for welded joints in machinery and equipment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006256043 / 2005-10-17
Date of Publication:
October 6, 2005
Date of Creation:
2005
Title:
AWS D14.4/D14.4M:2005, specification for welded joints in machinery and equipment.
Basis of Claim:
New Matter: new and rev. text, ill., and compilation.
Previous Registration:
Prev. reg. 1997, TX 4-523-871.
Copyright Note:
Cataloged from appl. only.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Laboratory methods for measuring fume generation rates and total fume emission of welding and allied processes
example document: Laboratory methods for measuring fume generation rates and total fume emission of welding and allied processes
Specification for aluminum brazing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0006267384 / 2005-10-05
Date of Publication:
September 5, 2011
Date of Creation:
2005
Title:
Specification for aluminum brazing : AWS C3.7M/C3.7:2005.
Basis of Claim:
New Matter: additions, revisions & compilation.
Previous Registration:
Prev. reg. 1999, TX 4-991-873.
Copyright Note:
Cataloged from appl. only.
Number of similar titles:
2
Copyright Claimant:
American Welding Society
Names:
American Welding Society (599 documents)
example document: Specification for carbon steel electrodes and fluxes for submerged arc welding
example document: Specification for carbon steel electrodes and fluxes for submerged arc welding
This website is not affiliated with document authors or copyright owners. This page is provided for informational purposes only. Unintentional errors are possible. Multiple persons can share the same name.