Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root followed by shielded metal arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN309, ER309, and E309-15, -16, or -17, or IN309, ER309(L), and ER309(L)-15, -16, or -17, As-welded condition, primarily pipe applications part 3
Metric practice guide for the welding industry
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005670038 / 2002-07-15
Date of Publication:
December 4, 2001
Date of Creation:
2001
Title:
Metric practice guide for the welding industry : AWS A1.1:2001, an American national standard.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 1998, TX 4-768-053.
Copyright Note:
C.O. correspondence.
Description:
32 p.
Variant title:
Metric practice guide for the welding industry : AWS A1.1:2001, an American national standard.
Copyright Claimant:
American Welding Society
Names:
American Welding Society
|
|
Standard welding procedure specification (WPS) for gas tungsten arc welding followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, ER3XX and E3XX-XX, as-welded condition, primarily plate and structural applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005701760 / 2002-01-28
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, ER3XX and E3XX-XX, as-welded condition, primarily plate and structural applications : an American national standard : AWS B2.1-8-025:2001.
Basis of Claim:
New Matter: added & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2000, TX 5-355-641.
Copyright Note:
C.O. correspondence.
Description:
18 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding followed by shielded metal arc welding
Other Title:
AWS B2.1-8-025:2001.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for friction welding
example document: Recommended practices for friction welding
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert root followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN3XX, ER3XX, and E3XX-XX, as-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005701761 / 2002-01-28
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert root followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN3XX, ER3XX, and E3XX-XX, as-welded condition, primarily pipe applications : an American national standard : AWS B2.1-8-216:2001.
Basis of Claim:
New Matter: added & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2000, TX 5-355-642.
Copyright Note:
C.O. correspondence.
Description:
17 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert root followed
Other Title:
AWS B2.1-8-216:2001.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for bare aluminum and aluminum alloy welding electrodes and rods substances
example document: Specification for bare aluminum and aluminum alloy welding electrodes and rods substances
Standard welding procedure specification (WPS) for gas tungsten arc welding followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, ER3XX and E3XX-XX, as-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005701762 / 2002-01-28
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, ER3XX and E3XX-XX, as-welded condition, primarily pipe applications : an American national standard : AWS B2.1-8-214:2001.
Basis of Claim:
New Matter: added & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2000, TX 5-355-637.
Copyright Note:
C.O. correspondence.
Description:
15 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding followed by shielded metal arc welding of
Other Title:
AWS B2.1-8-214:2001.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Standard welding procedures specification (WPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, E3XX-XX as-welded condition, primarily pipe applications
example document: Standard welding procedures specification (WPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, E3XX-XX as-welded condition, primarily pipe applications
Standard welding procedure specification (WPS) for gas tungsten arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/16 through 1-1/2 inch thick, ER3XX, as-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005701763 / 2002-01-28
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/16 through 1-1/2 inch thick, ER3XX, as-welded condition, primarily pipe applications : an American national standard : AWS B2.1-8-212:2001.
Basis of Claim:
New Matter: added & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2000, TX 5-355-638.
Copyright Note:
C.O. correspondence.
Description:
14 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding of austenitic stainless steel (M-8/P-8/S-8
Other Title:
AWS B2.1-8-212:2001.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for carbon steel electrodes and fluxes for submerged arc welding
example document: Specification for carbon steel electrodes and fluxes for submerged arc welding
Standard welding procedure specification (WPS) for gas tungsten, arc welding with consumable insert root of carbon steel ..
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005705671 / 2002-01-28
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten, arc welding with consumable insert root of carbon steel ...
Basis of Claim:
New Matter: new and rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2000, TX 5-355-640.
Copyright Note:
C.O. correspondence.
Series:
AWS B2.1-8-02-2001
Description:
16 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten, arc welding with consumable insert
Copyright Claimant:
American Welding Society
Names:
Standard welding procedure specification (WPS) for gas tungsten, arc welding of austenitic stainless steel ..
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005705672 / 2002-01-28
Date of Publication:
January 21, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (WPS) for gas tungsten, arc welding of austenitic stainless steel ...
Basis of Claim:
New Matter: new and rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 2000, TX 5-355-644.
Copyright Note:
C.O. correspondence.
Series:
AWS B2.1-8-024:2001
Description:
18 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for root pass welding of pipe without backing
example document: Recommended practices for root pass welding of pipe without backing
Specification for thermal spraying zinc anodes on steel reinforced concrete
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005756379 / 2003-03-18
Date of Publication:
March 6, 2003
Date of Creation:
2003
Title:
Specification for thermal spraying zinc anodes on steel reinforced concrete : AWS C2.20/C2.20M:2002.
Description:
27 p.
Other Title:
AWS C2.20/C2.20M:2002
Copyright Claimant:
American Welding Society
Names:
Guide for the joining of wrought nickel-based alloys
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005788635 / 2003-03-07
Date of Publication:
February 12, 2003
Date of Creation:
2003
Title:
Guide for the joining of wrought nickel-based alloys : AWS G2.1M/G2.1:2002.
Description:
48 p.
Variant title:
Guide for the joining of wrought nickel-based alloys : AWS G2.1M/G2.1:2002.
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Structural welding code--aluminum
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005826523 / 2003-05-22
Date of Publication:
May 13, 2003
Date of Creation:
2003
Title:
Structural welding code--aluminum : an American National Standard AWS D1.2/D1.2M:2003.
Edition:
4th ed.
Basis of Claim:
New Matter: additional text, compilation of data, rev. text & ill.
Previous Registration:
Prev. reg. 1997, TX 4-597-860.
Imprint:
Miami : AWS, c2003.
Description:
201 p.
Other Title:
AWS D1.2/D1.2M:2003
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for metal cutting machine tool weldments
example document: Specification for metal cutting machine tool weldments
Guide for thermal-spray operator qualification
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005852787 / 2002-11-25
Date of Publication:
November 18, 2002
Date of Creation:
2002
Title:
Guide for thermal-spray operator qualification : AWS C2.16/C2.16M:2002, an American national standard.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 1992, TX 3-504-672.
Description:
75 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for friction welding
example document: Recommended practices for friction welding
Specification for the qualification of radiographic interpreters
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005852839 / 2003-05-15
Date of Publication:
May 5, 2003
Date of Creation:
2003
Title:
Specification for the qualification of radiographic interpreters : AWS B5.15:2003, an American national standard.
Description:
8 p.
Variant title:
Specification for the qualification of radiographic interpreters : AWS B5.15:2003, an American national standard.
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Specification for the qualification of welding sales representatives
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005853481 / 2002-10-15
Date of Publication:
October 8, 2002
Date of Creation:
2002
Title:
Specification for the qualification of welding sales representatives : AWS B5.14:2002 : an American National Standard.
Description:
1 v.
Variant title:
Specification for the qualification of welding sales representatives : AWS B5.14:2002
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Laboratory method for measuring fume generation rates and total fume emission of welding and allied processes
example document: Laboratory method for measuring fume generation rates and total fume emission of welding and allied processes
Recommended practices for shielding gases for welding and cutting
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005857480 / 2003-10-30
Date of Publication:
October 23, 2003
Date of Creation:
2003
Title:
Recommended practices for shielding gases for welding and cutting : AWS C5.10/C5.10M:2003.
Description:
53 p.
Variant title:
Recommended practices for shielding gases for welding and cutting : AWS C5.10/C5.10M:2003.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for ultrasonic inspection of brazed joints
example document: Recommended practices for ultrasonic inspection of brazed joints
Standard welding procedure specification (SWPS) for gas tungsten arc welding of aluminum (M/P/S-22 to M/P/S-22), 18 through 10 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859926 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of aluminum (M/P/S-22 to M/P/S-22), 18 through 10 gauge, in the as-welded condition, with or without backing : AWS B2.1-22-015:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1992, TX 3-372-692.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of aluminum (M/P/S-22 to M/P/S-22)
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Standard welding procedures specification (WPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, E3XX-XX as-welded condition, primarily pipe applications
example document: Standard welding procedures specification (WPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, E3XX-XX as-welded condition, primarily pipe applications
Standard welding procedure specification (SWPS) for shielded metal arc welding of carbon steel to austenitic stainless steel (M-1 to M-8/P-8/S-8, group 1), 10 through 17 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859927 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for shielded metal arc welding of carbon steel to austenitic stainless steel (M-1 to M-8/P-8/S-8, group 1), 10 through 17 gauge, in the as-welded condition, with or without backing : AWS B2.1-1/8-014:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1992, TX 3-372-691.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for shielded metal arc welding of carbon steel
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Metric practice guide for the welding industry
example document: Metric practice guide for the welding industry
Standard welding procedure specification (SWPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 10 through 18 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859928 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 10 through 18 gauge, in the as-welded condition, with or without backing : AWS B2.1-8-013:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for shielded metal arc welding of austenitic stainless steel
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard welding procedure specification (SWPS) for shielded metal arc welding of carbon steel (M-1, P-1, or S-1 to M-1, P-1, or S-1), 10 through 18 guage, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859929 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for shielded metal arc welding of carbon steel (M-1, P-1, or S-1 to M-1, P-1, or S-1), 10 through 18 guage, in the as-welded condition, with or without backing : AWS B2.1-1-012:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. TX 3-370-035, 1992.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for shielded metal arc welding of carbon steel
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard welding procedure specificationi (SWPS) for shielded metal arc welding of galvanized stainless steel (M-1), 10 through 18 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859930 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specificationi (SWPS) for shielded metal arc welding of galvanized stainless steel (M-1), 10 through 18 gauge, in the as-welded condition, with or without backing : AWS B2.1-1-011:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1992, TX 3-338-192.
Description:
12 p.
Variant title:
Standard welding procedure specificationi (SWPS) for shielded metal arc welding of galvanized stainless steel (M-1)
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard welding procedure specificationi (SWPS) for gas tungsten arc welding of carbon steel to austenitic stainless steel (M-1), P-1, or S-1 to M-8, P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859931 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specificationi (SWPS) for gas tungsten arc welding of carbon steel to austenitic stainless steel (M-1), P-1, or S-1 to M-8, P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing : AWS B2.1-1/8-010:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1990, TX 2-855-622.
Description:
12 p.
Variant title:
Standard welding procedure specificationi (SWPS) for gas tungsten arc welding of carbon steel
Copyright Claimant:
American Welding Society
Names:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of austenitic stainless steel (M-8), P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859932 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of austenitic stainless steel (M-8), P-8, or S-8), 18 through 10 gauge, in the as-welded condition, with or without backing : AWS B2.1-8-009:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1990, TX 2-855-625.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of austenitic stainless steel
Copyright Claimant:
American Welding Society
Names:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of carbon steel (M-1, P-1, or S-1), 18 through 10 gauge, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005859933 / 2003-10-22
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of carbon steel (M-1, P-1, or S-1), 18 through 10 gauge, in the as-welded condition, with or without backing : AWS B2.1-1-008:2002 : an American national standard.
Basis of Claim:
New Matter: additions, revisions, compilation.
Previous Registration:
Prev. reg. 1990, TX 2-839-084.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of carbon steel
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for aluminum and aluminum alloy electrodes for shielded metal arc welding
example document: Specification for aluminum and aluminum alloy electrodes for shielded metal arc welding
Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/16 through 1-1/2 inch thick, IN309 and ER309(L), As-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005873020 / 2002-11-14
Date of Publication:
November 8, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/16 through 1-1/2 inch thick, IN309 and ER309(L), As-welded condition, primarily pipe applications : an American national standard : AWS B2.1-1/8-230:2002.
Description:
14 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root of carbon steel
Copyright Claimant:
American Welding Society
Names:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/16 through 1-1/2 inch thick, ER309(L), As-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005873021 / 2002-11-14
Date of Publication:
November 8, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/16 through 1-1/2 inch thick, ER309(L), As-welded condition, primarily pipe applications : an American national standard : AWS B2.1-1/8-227:2002.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding of carbon steel
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices and procedures for welding low carbon steel pipe
example document: Recommended practices and procedures for welding low carbon steel pipe
Standard welding procedure specification (SWPS) for Shielded metal arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, E309(L)-15, -16, or 17, As-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005873022 / 2002-11-14
Date of Publication:
November 8, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for Shielded metal arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, E309(L)-15, -16, or 17, As-welded condition, primarily pipe applications : an American national standard : AWS B2.1-1/8-228:2002.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for Shielded metal arc welding of carbon steel
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard welding procedure specification (SWPS) for gas tungsten arc welding followed by shielded metal arc of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, ER309(L) and E309(L)-15, -16, or -17, As-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005873023 / 2002-11-14
Date of Publication:
November 8, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding followed by shielded metal arc of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, ER309(L) and E309(L)-15, -16, or -17, As-welded condition, primarily pipe applications : an American national standard : AWS B2.1-1/8-229:2002.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding followed by shielded metal arc
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Operator's manual for oxyfuel gas cutting
example document: Operator's manual for oxyfuel gas cutting
Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root followed by shielded metal arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN309, ER309, and E309-15, -16, or -17, or IN309, ER309(L), and ER309(L)-15, -16, or -17, As-welded condition, primarily pipe applications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005873024 / 2002-11-14
Date of Publication:
November 8, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root followed by shielded metal arc welding of carbon steel (M-1/P-1/S-1, groups 1 or 2) to austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN309, ER309, and E309-15, -16, or -17, or IN309, ER309(L), and ER309(L)-15, -16, or -17, As-welded condition, primarily pipe applications : an American national standard : AWS B2.1-1/8-231:2002.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas tungsten arc welding with consumable insert root
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Standard procedures for calibrating magnetic instruments to measure the Delta ferrite content of austenitic stainless steel weld metal
example document: Standard procedures for calibrating magnetic instruments to measure the Delta ferrite content of austenitic stainless steel weld metal
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of galvanized steel (M-1), 18 through 10 gage, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005881091 / 2003-01-06
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of galvanized steel (M-1), 18 through 10 gage, in the as-welded condition, with or without backing : AWS B2.1-1-003:2002.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 1990, TX 2-855-621.
Copyright Note:
C.O. correspondence.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode)
Copyright Claimant:
American Welding Society
Notes:
Supersedes ANSI/AWS B2.1.003-90.
Names:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of carbon steel (M-1, group 1), 18 through 10 gage, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005881092 / 2003-01-06
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of carbon steel (M-1, group 1), 18 through 10 gage, in the as-welded condition, with or without backing : AWS B2.1-1-004:2002.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 1990, TX 2-855-619.
Copyright Note:
C.O. correspondence.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode)
Copyright Claimant:
American Welding Society
Notes:
Supersedes ANSI/AWS B2.1-1-004-90.
Names:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of austenitic stainless steel (M-8, P-8, or S-8), 18 through 10 gage, in the as-welded condition, with or without backing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0005881093 / 2003-01-06
Date of Publication:
October 11, 2002
Date of Creation:
2002
Title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode) of austenitic stainless steel (M-8, P-8, or S-8), 18 through 10 gage, in the as-welded condition, with or without backing : AWS B2.1-8-005:2002.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation.
Previous Registration:
Prev. reg. 1990, TX 2-855-626.
Copyright Note:
C.O. correspondence.
Description:
12 p.
Variant title:
Standard welding procedure specification (SWPS) for gas metal arc welding (short circuiting transfer mode)
Copyright Claimant:
American Welding Society
Notes:
Supersedes ANSI/AWS B2.1.005-90.
Names:
American Welding Society (362 documents)
example document: Guide for thermal spray operator and equipment qualification
example document: Guide for thermal spray operator and equipment qualification