Standard welding procedure specification (WPS) for Gas tungsten arc welding (consumable insert root) followed by shielded metal arc welding of chromium-molybdenum steel (M-4/P-4, group 1 or 2), 1/8 through 1/2 in. thick as-welded condition, 1/8 through 1-1/2 in thick, PWHT condition, IN515, ER80S-B2, and E8018-B2, primary pipe applications part 2
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2) 1/8 through 1-1/2 inch thick, E6010 (vertical uphill) followed by E7018 (vertical uphill) as-welded or PWHT condition
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004462997 / 1997-04-29
Date of Publication:
October 14, 1996
Date of Creation:
1996
Title:
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2) 1/8 through 1-1/2 inch thick, E6010 (vertical uphill) followed by E7018 (vertical uphill) as-welded or PWHT condition : ANSI/AWS B2.1-1-205-96.
Description:
8 p.
Variant title:
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel
Other Title:
ANSI/AWS B2.1-1-205-96
Copyright Claimant:
American Welding Society (employer for hire in text, compilation of data & ill.)
Notes:
An American national standard.
Names:
American Welding Society (362 documents)
example document: Standard procedures for determination of moisture content of welding fluxes and welding electrode flux coverings
example document: Standard procedures for determination of moisture content of welding fluxes and welding electrode flux coverings
|
|
Standard welding procedure specification (WPS) sheilded metal arc welding of carbon steel
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004471810 / 1997-04-29
Date of Publication:
October 14, 1996
Date of Creation:
1996
Title:
Standard welding procedure specification (WPS) sheilded metal arc welding of carbon steel : (M-1/P-1/S-1, group 1 or 1) 1/8 through 1/-1/2 inch thick, E6010 (vertical downhill) followed by E7018 (vertical uphill) as-welded or PWHT condition.
Description:
1 v.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Operator's manual for oxyfuel gas cutting
example document: Operator's manual for oxyfuel gas cutting
Recommended practices for welding of chromium-molybdenum steel piping and tubing
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004516903 / 1997-04-29
Date of Publication:
December 10, 1996
Date of Creation:
1996
Title:
Recommended practices for welding of chromium-molybdenum steel piping and tubing : an American national standard ANSI/AWS D10.8-96.
Basis of Claim:
New Matter: added & rev. text, compilation & ill.
Previous Registration:
Prev. reg.
Description:
12 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Standard procedures for calibrating magnetic instruments to measure the delta ferrite content of austenitic and duplex austenitic-ferritic stainless steel weld metal
example document: Standard procedures for calibrating magnetic instruments to measure the delta ferrite content of austenitic and duplex austenitic-ferritic stainless steel weld metal
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2) 1/8 through 3/4 inch thick, E6010 (vertical uphill) followed by E7018 (vertical uphill) as-welded condition
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004523837 / 1997-04-29
Date of Publication:
October 14, 1996
Date of Creation:
1996
Title:
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2) 1/8 through 3/4 inch thick, E6010 (vertical uphill) followed by E7018 (vertical uphill) as-welded condition : ANSI/AWS B2.1-1-201-96.
Description:
7 p.
Variant title:
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2)
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for automotive weld quality-resistance spot welding
example document: Recommended practices for automotive weld quality-resistance spot welding
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2) 1/8 through 3/4 inch thick, E6010 (vertical downhill) followed by E7018 (vertical uphill) as-welded condition
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004523838 / 1997-04-29
Date of Publication:
October 14, 1996
Date of Creation:
1996
Title:
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2) 1/8 through 3/4 inch thick, E6010 (vertical downhill) followed by E7018 (vertical uphill) as-welded condition : ANSI/AWS B2.1-1-201-96.
Description:
7 p.
Variant title:
Standard welding procedure specification (WPS) shielded metal arc welding of carbon steel (M-1/P-1/S-1, group 1 or 2)
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Specification for welded joints in machinery and equipment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004523871 / 1997-04-29
Date of Publication:
February 10, 1997
Date of Creation:
1997
Title:
Specification for welded joints in machinery and equipment : ANSI/AWS D14.4-97.
Description:
127 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for welding sheet steel in structures
example document: Specification for welding sheet steel in structures
Methods for sampling and analyzing gases from welding and allied processes
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004523872 / 1997-04-29
Date of Publication:
January 9, 1997
Date of Creation:
1997
Title:
Methods for sampling and analyzing gases from welding and allied processes : ANSI/AWS F1.5-96.
Description:
37 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for gas shielded arc welding of aluminum and aluminum alloy pipe
example document: Recommended practices for gas shielded arc welding of aluminum and aluminum alloy pipe
Bridge welding code
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004532176 / 1997-04-29
Date of Publication:
January 9, 1997
Date of Creation:
1996
Title:
Bridge welding code : ANSI/AASHTO/AWS D1.5-96.
Basis of Claim:
New Matter: compilation, revisions & additions, ill.
Previous Registration:
Prev. reg. 1995.
Description:
230 p.
Variant title:
Bridge welding code : ANSI/AASHTO/AWS D1.5-96
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Operators manual for oxyfuel gas heating torch operation
example document: Operators manual for oxyfuel gas heating torch operation
Methods for analysis of airborne particulates generated by welding and allied processes
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004597767 / 1997-10-24
Date of Publication:
May 27, 1997
Date of Creation:
1997
Title:
Methods for analysis of airborne particulates generated by welding and allied processes : ANSI/AWS F1.4--1997.
Basis of Claim:
New Matter: new text, ill. & compilation.
Previous Registration:
Prev. reg. 1987, TX 2-157-156.
Description:
18 p.
Copyright Claimant:
American Welding Society
Names:
Specification for welding of presses and press components
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004597862 / 1997-10-24
Date of Publication:
August 20, 1997
Date of Creation:
1997
Title:
Specification for welding of presses and press components / ANSI/AWS D14.5--97. prepared by AWS Committee on Machinery and Equipment :
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg.
Description:
146 p.
Other Title:
American Welding Society. Committee on Machinery and Equipment
Copyright Claimant:
American Welding Society (employer for hire)
Names:
American Welding Society
Specification for consumable inserts
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004678850 / 1997-12-03
Date of Publication:
November 25, 1997
Date of Creation:
1997
Title:
Specification for consumable inserts : ANSI/AWS A5.30-97.
Basis of Claim:
New Matter: added & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg.
Description:
23 p.
Other Title:
ANSI/AWS A5.30-97
Copyright Claimant:
American Welding Society
Names:
Recommended practices for test methods for evaluating the resistance spot welding behavior of automotive sheet steel materials
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004693364 / 1997-12-02
Date of Publication:
November 24, 1997
Date of Creation:
1997
Title:
Recommended practices for test methods for evaluating the resistance spot welding behavior of automotive sheet steel materials : ANSI/AWS/SAE/D8.9-97, an American national standard.
Description:
55 p.
Variant title:
Recommended practices for test methods for evaluating the resistance spot welding behavior
Copyright Claimant:
American Welding Society
Names:
Specification for welding shielding gases
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004716052 / 1998-02-02
Date of Publication:
January 27, 1998
Date of Creation:
1998
Title:
Specification for welding shielding gases : ANSI/AWS A5.32/A5.32M-97.
Description:
19 p.
Variant title:
Specification for welding shielding gases : ANSI/AWS A5.32/A5.32M-97.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specifications for use and performance of transparent welding curtains and screens
example document: Specifications for use and performance of transparent welding curtains and screens
Structural welding code--reinforcing steel
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004731541 / 1998-02-23
Date of Publication:
February 17, 1998
Date of Creation:
1998
Title:
Structural welding code--reinforcing steel : ANSI/AWS D1.4-98.
Basis of Claim:
New Matter: additions, compilation, revisions.
Previous Registration:
Prev. reg. 1992, TX 3-431-833.
Imprint:
Miami : American Welding Society, c1998.
Description:
45 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard symbols for welding, brazing, and nondestructive examination
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004732600 / 1998-03-09
Date of Publication:
February 27, 1998
Date of Creation:
1998
Title:
Standard symbols for welding, brazing, and nondestructive examination : ANSI/AWS A2.4-98.
Basis of Claim:
New Matter: compilation, revisions & additions.
Previous Registration:
Prev. reg. 1993, TX 3-619-478.
Imprint:
Miami : American Welding Society, c1998.
Description:
109 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for welding of chromium-molybdenum steel piping and tubing
example document: Recommended practices for welding of chromium-molybdenum steel piping and tubing
Specification for carbon steel electrodes and fluxes for submerged arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004742450 / 1998-03-16
Date of Publication:
March 10, 1998
Date of Creation:
1998
Title:
Specification for carbon steel electrodes and fluxes for submerged arc welding : ANSI/AWS A5.17/A5.17M-97.
Basis of Claim:
New Matter: new & rev. text, ill. & compilation of data.
Previous Registration:
Prev. reg. 1989, TX 2-700-440.
Description:
31 p.
Variant title:
Specification for carbon steel electrodes and fluxes for submerged arc welding : ANSI/AWS A5.17/A5.17M-97.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for welding of chromium-molybdenum steel piping and tubing
example document: Recommended practices for welding of chromium-molybdenum steel piping and tubing
Specification for tungsten and tungsten-alloy electrodes for arc welding and cutting
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004764408 / 1998-04-24
Date of Publication:
April 13, 1998
Date of Creation:
1998
Title:
Specification for tungsten and tungsten-alloy electrodes for arc welding and cutting : ANSI/AWS A5.12/A5.12M-98.
Basis of Claim:
New Matter: new & rev. text, ill.; compilation of data.
Previous Registration:
Prev. reg. 1992, TX 3-577-961.
Description:
15 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices and procedures for welding low carbon steel pipe
example document: Recommended practices and procedures for welding low carbon steel pipe
Specification for carbon and low-alloy steel electrodes for electrogas welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004776966 / 1998-05-20
Date of Publication:
May 8, 1998
Date of Creation:
1998
Title:
Specification for carbon and low-alloy steel electrodes for electrogas welding : ANSI/AWS A5.26/A5.26M-97.
Basis of Claim:
New Matter: revisions, compilation, additions.
Previous Registration:
Prev. reg. 1992, TX 3-323-857.
Description:
27 p.
Copyright Claimant:
American Welding Society
Names:
Specification for carbon and low-alloy steel electrodes for fluxes for electroslag welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004776967 / 1998-05-20
Date of Publication:
May 7, 1998
Date of Creation:
1998
Title:
Specification for carbon and low-alloy steel electrodes for fluxes for electroslag welding : ANSI/AWS A5.25/A5.25M-97.
Basis of Claim:
New Matter: revisions, compilation, additions.
Previous Registration:
Prev. reg. 1992, TX 3-323-858.
Description:
27 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for copper and copper alloy rods for oxyfuel gas welding
example document: Specification for copper and copper alloy rods for oxyfuel gas welding
Specification for nickel and nickel-alloy welding electrodes for shielded metal arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004776968 / 1998-05-20
Date of Publication:
May 8, 1998
Date of Creation:
1998
Title:
Specification for nickel and nickel-alloy welding electrodes for shielded metal arc welding : ANSI/AWS A5.11/A5.11M-97.
Basis of Claim:
New Matter: revisions, compilation, additions.
Previous Registration:
Prev. reg. 1991, TX 3-112-158.
Description:
27 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard methods for mechanical testing of welds
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004776969 / 1998-05-20
Date of Publication:
May 11, 1998
Date of Creation:
1998
Title:
Standard methods for mechanical testing of welds : ANSI/AWS B4.0-98.
Basis of Claim:
New Matter: revisions, compilation, additions.
Previous Registration:
Prev. reg. 1993, TX 3-510-199.
Description:
98 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Operators manual for oxyfuel gas heating torch operation
example document: Operators manual for oxyfuel gas heating torch operation
Specification for low-alloy steel electrodes and fluxes for submerged arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004845369 / 1998-08-05
Date of Publication:
July 27, 1998
Date of Creation:
1998
Title:
Specification for low-alloy steel electrodes and fluxes for submerged arc welding : ANSI/AWS A5.23/A5.23M-1997.
Basis of Claim:
New Matter: new & rev. text, ill., & compilation of data.
Previous Registration:
Prev. reg. 1990, TX 2-847-583.
Description:
37 p.
Variant title:
Specification for low-alloy steel electrodes and fluxes for submerged arc welding : ANSI/AWS A5.23/A5.23M-1997.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Recommended practices for gas shielded arc welding of aluminum and aluminum alloy pipe
example document: Recommended practices for gas shielded arc welding of aluminum and aluminum alloy pipe
Specification for low-alloy steel electrodes for flux cored arc welding
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004850874 / 1998-09-08
Date of Publication:
September 1, 1998
Date of Creation:
1998
Title:
Specification for low-alloy steel electrodes for flux cored arc welding : ANSI/AWS 5.29:1998.
Basis of Claim:
New Matter: revisions, additions & compilation.
Previous Registration:
Prev. reg.
Description:
39 p.
Variant title:
Specification for low-alloy steel electrodes for flux cored arc welding : ANSI/AWS 5.29:1998
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN3XX, ER3XXX, and E3XX-XX, as-welded condition
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004864692 / 1998-10-20
Date of Publication:
October 16, 1998
Date of Creation:
1998
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert followed by shielded metal arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN3XX, ER3XXX, and E3XX-XX, as-welded condition : ANSI/AWS B2.1-8-216:1998.
Description:
15 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert
Other Title:
ANSI/AWS B2.1-8-216:1998.
Copyright Claimant:
American Welding Society
Names:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN3XX and ER3XX, as-welded condition
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004876747 / 1998-10-19
Date of Publication:
October 16, 1998
Date of Creation:
1998
Title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert of austenitic stainless steel (M-8/P-8/S-8, group 1), 1/8 through 1-1/2 inch thick, IN3XX and ER3XX, as-welded condition : abstract : ANSI/AWS B2.1-8-215:1998, an American national standard / prepared by AWS. Committee on Welding Qualification.
Description:
15 p.
Variant title:
Standard welding procedure specification (WPS) for gas tungsten arc welding with consumable insert
Copyright Claimant:
American Welding Society (employer for hire)
Names:
AWS. Committee on Welding Qualification (3 documents)
example document: Standard welding procedures specification (WPS) for gas tungsten arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, ER3XX as-welded condition, primarily pipe applications
American Welding Society
example document: Standard welding procedures specification (WPS) for gas tungsten arc welding of austenitic stainless steel (M-8/P-8/S-8, group 1) 1/8 through 1-1/2 inch thick, ER3XX as-welded condition, primarily pipe applications
American Welding Society
International index of welding filler metal classifications
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004894819 / 1998-11-27
Date of Publication:
November 16, 1998
Date of Creation:
1998
Title:
International index of welding filler metal classifications.
Imprint:
Miami : American Welding Society, c1998.
Description:
64 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for automotive frame weld quality--arc welding
example document: Specification for automotive frame weld quality--arc welding
Effects of welding on health
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004920775 / 1999-01-12
Date of Publication:
January 6, 1999
Date of Creation:
1999
Title:
Effects of welding on health : index, I through X.
Description:
41 p.
Variant title:
Effects of welding on health : index, I through X.
Copyright Claimant:
American Welding Society
Names:
American Welding Society
Safety and health fact sheets
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004927828 / 1999-01-25
Date of Publication:
January 19, 1999
Date of Creation:
1999
Title:
Safety and health fact sheets.
Edition:
2nd ed.
Description:
1 v.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Standard procedures for calibrating magnetic instruments to measure the Delta ferrite content of austenitic stainless steel weld metal
example document: Standard procedures for calibrating magnetic instruments to measure the Delta ferrite content of austenitic stainless steel weld metal
Safety in welding, cutting, and allied processes
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004957558 / 1999-03-04
Date of Publication:
March 2, 1999
Date of Creation:
1999
Title:
Safety in welding, cutting, and allied processes.
Basis of Claim:
New Matter: new and rev. text, ill, and compilation.
Previous Registration:
Prev. reg. 1995, TX 4-035-139.
Series:
ANSI Z49.1:1999
Description:
52 p.
Copyright Claimant:
American Welding Society
Notes:
An American national standard.
Names:
American Welding Society
Structural welding code--stainless steel
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0004989040 / 1999-05-21
Date of Publication:
May 17, 1999
Date of Creation:
1999
Title:
Structural welding code--stainless steel : AWS D1.6:1999 an American national standard.
Description:
210 p.
Copyright Claimant:
American Welding Society
Names:
American Welding Society (362 documents)
example document: Specification for carbon steel electrodes and fluxes for submerged arc welding
example document: Specification for carbon steel electrodes and fluxes for submerged arc welding