Welding procedure specification number 4:3-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel with insert followed by E8018-B2 without postweld heat treatment
Welding procedure specification number 4:3-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel with insert followed by E8018-B2 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580696 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:3-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel with insert followed by E8018-B2 with postweld heat treatment.
Variant title:
Welding procedure specification number 4:3-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 21.13 for gas tungsten arc welding (G T A W) of austenitic pipe, valves, fittings, and flanges
example document: Welding procedure specification number 21.13 for gas tungsten arc welding (G T A W) of austenitic pipe, valves, fittings, and flanges
|
|
Welding procedure specification number 51-3-1 for gas tungsten arc welding of P-51 titanium using ERTi-2 filler metal
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580697 / 1988-08-24
Date of Publication:
July 10, 1987
Date of Creation:
1988
Title:
Welding procedure specification number 51-3-1 for gas tungsten arc welding of P-51 titanium using ERTi-2 filler metal.
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 8:1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of austenitic stainless steel to carbon steel using insert followed by E309 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580698 / 1988-08-24
Date of Publication:
May 25, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 8:1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of austenitic stainless steel to carbon steel using insert followed by E309 without postweld heat treatment.
Variant title:
Welding procedure specification number 8:1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 45.12 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of nickel base alloy pipe, valves, fittings, and flanges (carpenter 20)
example document: Welding procedure specification number 45.12 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of nickel base alloy pipe, valves, fittings, and flanges (carpenter 20)
Welding procedure specification number 4:3-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel with insert followed by E8018-B2 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580699 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:3-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel with insert followed by E8018-B2 without postweld heat treatment.
Variant title:
Welding procedure specification number 4:3-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings, and flanges using E7018 with or without postweld heat treatment
example document: Welding procedure specification number 1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings, and flanges using E7018 with or without postweld heat treatment
Welding procedure specification number 4:1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580700 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 with postweld heat treatment.
Basis of Claim:
New Matter: updating.
Previous Registration:
Prev. reg. 1977 as Welding procedure specification number 4.11.
Variant title:
Welding procedure specification number 4:1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Other Title:
Welding procedure specification number 4.11.
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification no. 4-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using E8018-B2 with postweld heat treatment
example document: Welding procedure specification no. 4-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using E8018-B2 with postweld heat treatment
Welding procedure specification number 5:1-42-3 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon with insert followed by E502 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580701 / 1988-08-24
Date of Publication:
May 4, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 5:1-42-3 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon with insert followed by E502 with postweld heat treatment.
Variant title:
Welding procedure specification number 5:1-42-3 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 5:3-2-1 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E9018-B3 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580702 / 1988-08-24
Date of Publication:
May 4, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 5:3-2-1 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E9018-B3 with postweld heat treatment.
Variant title:
Welding procedure specification number 5:3-2-1 for shielded metal arc welding (S M A W)
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification
example document: Welding procedure specification
Welding procedure specification number 8:4-2-1 for shielded metal arc welding (S M A W) of austenitic stainless steel to P4 chromium molybdenum steel using E309-16 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580703 / 1988-08-24
Date of Publication:
May 5, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 8:4-2-1 for shielded metal arc welding (S M A W) of austenitic stainless steel to P4 chromium molybdenum steel using E309-16 without postweld heat treatment.
Variant title:
Welding procedure specification number 8:4-2-1 for shielded metal arc welding (S M A W)
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-37-1 for gas tungsten arc welding (G T A W) and gas metal arc welding (S A W) with fluxcore wire (G M A W-F C), manual of [i.e. or] semi-automatic of carbon steel without consumable insert and without postweld heat treatment
example document: Welding procedure specification number 1-37-1 for gas tungsten arc welding (G T A W) and gas metal arc welding (S A W) with fluxcore wire (G M A W-F C), manual of [i.e. or] semi-automatic of carbon steel without consumable insert and without postweld heat treatment
Welding procedure specification number 8:1-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of austenitic stainless steel to carbon steel using F43 filler metal without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580704 / 1988-08-24
Date of Publication:
May 5, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 8:1-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of austenitic stainless steel to carbon steel using F43 filler metal without postweld heat treatment.
Variant title:
Welding procedure specification number 8:1-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 5:3-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E9018-B3 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580705 / 1988-08-24
Date of Publication:
May 4, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 5:3-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E9018-B3 without postweld heat treatment.
Variant title:
Welding procedure specification number 5:3-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 4-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using E8018-B2 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580706 / 1988-08-24
Date of Publication:
April 30, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using E8018-B2 without postweld heat treatment.
Variant title:
Welding procedure specification number 4-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1.13 for shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings and flanges using iron power, low hydrogen electrodes with preheat and postweld heat treatment
example document: Welding procedure specification number 1.13 for shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings and flanges using iron power, low hydrogen electrodes with preheat and postweld heat treatment
Welding procedure specification number 4-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using insert followed by E8018-B2 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580707 / 1988-08-24
Date of Publication:
April 30, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using insert followed by E8018-B2 with postweld heat treatment.
Variant title:
Welding procedure specification number 4-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel using insert followed by E7018 with or without postweld heat treatment
example document: Welding procedure specification number 1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel using insert followed by E7018 with or without postweld heat treatment
Welding procedure specification number 4-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using insert followed by E8018-B2 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580708 / 1988-08-24
Date of Publication:
April 30, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel using insert followed by E8018-B2 without postweld heat treatment.
Variant title:
Welding procedure specification number 4-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 4:1-2-1 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580709 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:1-2-1 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 with postweld heat treatment.
Variant title:
Welding procedure specification number 4:1-2-1 for shielded metal arc welding (S M A W)
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification
example document: Welding procedure specification
Welding procedure specification number 4:1-2-2 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580710 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:1-2-2 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 without postweld heat treatment.
Variant title:
Welding procedure specification number 4:1-2-2 for shielded metal arc welding (S M A W)
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 5:4-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of P5 chromium molybdenum steel to P4 chromium molybdenum steel using E9018-B3 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580711 / 1988-08-24
Date of Publication:
May 4, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 5:4-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of P5 chromium molybdenum steel to P4 chromium molybdenum steel using E9018-B3 without postweld heat treatment.
Variant title:
Welding procedure specification number 5:4-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-9-1 for oxyfuel gas welding (O F W) of carbon steel without postweld heat treatment
example document: Welding procedure specification number 1-9-1 for oxyfuel gas welding (O F W) of carbon steel without postweld heat treatment
Welding procedure specification number 4:1-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580712 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:1-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel using E8018-B2 without postweld heat treatment.
Variant title:
Welding procedure specification number 4:1-32-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 4:1-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel with insert followed by E8018-B2 without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580713 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:1-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel with insert followed by E8018-B2 without postweld heat treatment.
Variant title:
Welding procedure specification number 4:1-42-2 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 23.12 (re-numbered procedure 33B) for gas tungsten arc welding (G T A W) of aluminum pipe, valves, fittings, and flanges
example document: Welding procedure specification number 23.12 (re-numbered procedure 33B) for gas tungsten arc welding (G T A W) of aluminum pipe, valves, fittings, and flanges
Welding procedure specification number 4:1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel with insert followed by E8018-B2 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580714 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon steel with insert followed by E8018-B2 with postweld heat treatment.
Variant title:
Welding procedure specification number 4:1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Instructions for completing the record of welder/operator qualification test and selection and correct use of the uniform welder performance qualification test
example document: Instructions for completing the record of welder/operator qualification test and selection and correct use of the uniform welder performance qualification test
Welding procedure specification number 4:3-2-1 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E8018-B2 with postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580715 / 1988-08-24
Date of Publication:
May 1, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 4:3-2-1 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E8018-B2 with postweld heat treatment.
Variant title:
Welding procedure specification number 4:3-2-1 for shielded metal arc welding (S M A W)
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification 5.13 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) welding (S M A W) of P5 chromium molybdenum steel pipe, valves, fittings, and flanges to P1 carbon steel pipe, valves, fittings, and flanges
example document: Welding procedure specification 5.13 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) welding (S M A W) of P5 chromium molybdenum steel pipe, valves, fittings, and flanges to P1 carbon steel pipe, valves, fittings, and flanges
Welding procedure specification number 21-3-1 for gas tungsten arc welding (G T A W) of aluminum pipe using ER1100 filler metal
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580716 / 1988-08-24
Date of Publication:
May 25, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 21-3-1 for gas tungsten arc welding (G T A W) of aluminum pipe using ER1100 filler metal.
Basis of Claim:
New Matter: updating.
Previous Registration:
Prev. reg. 1975 as Welding procedure number 21.10.
Variant title:
Welding procedure specification number 21-3-1 for gas tungsten arc welding (G T A W) of aluminum pipe
Other Title:
Welding procedure number 21.10.
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-38-1 for gas tungsten arc welding (G T A W) and submerged arc welding (S A W), manual or machine of carbon steel without consumable insert
example document: Welding procedure specification number 1-38-1 for gas tungsten arc welding (G T A W) and submerged arc welding (S A W), manual or machine of carbon steel without consumable insert
Welding procedure specification number 8:5-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of austenitic stainless steel to P5 carbon molybdenum steel using F43 filler metal without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580717 / 1988-08-24
Date of Publication:
May 5, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 8:5-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of austenitic stainless steel to P5 carbon molybdenum steel using F43 filler metal without postweld heat treatment.
Variant title:
Welding procedure specification number 8:5-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau
Welding procedure specification number 8:5-2-1 for shielded metal arc welding (S M A W) of austenitic stainless steel to P5 chromium molybdenum steel using F-43 electrode without postweld heat treatment
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002580718 / 1988-08-24
Date of Publication:
May 5, 1987
Date of Creation:
1987
Title:
Welding procedure specification number 8:5-2-1 for shielded metal arc welding (S M A W) of austenitic stainless steel to P5 chromium molybdenum steel using F-43 electrode without postweld heat treatment.
Variant title:
Welding procedure specification number 8:5-2-1 for shielded metal arc welding (S M A W)
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings, and flanges using E7018 with or without postweld heat treatment
example document: Welding procedure specification number 1-32-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings, and flanges using E7018 with or without postweld heat treatment
Welding procedure specification
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002581492 / 1988-08-24
Date of Publication:
April 30, 1987
Date of Creation:
1987
Title:
Welding procedure specification : no. 4-2-2 : for shielded metal arc welding (S M A W) of chromium molybdenum steel pipe, valves, fittings, and flanges using E8018-B2 without postweld heat treatment.
Description:
4 p.
Variant title:
Welding procedure specification : no. 4-2-2
Copyright Claimant:
National Certified Pipe Welding Bureau
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel using insert followed by E7018 with or without postweld heat treatment
example document: Welding procedure specification number 1-42-1 for gas tungsten arc welding (G T A W) and shielded metal arc welding (S M A W) of carbon steel using insert followed by E7018 with or without postweld heat treatment
Welding procedure specification
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002581493 / 1988-08-24
Date of Publication:
May 4, 1987
Date of Creation:
1987
Title:
Welding procedure specification : no. 5:1-2-1 : for shielded metal arc welding (S M A W) of chromium molybdenum steel pipe, valves, fittings, and flanges to carbon steel pipe, valves, fittings, and flanges using E9018-B3 with postweld heat treatment.
Description:
4 p.
Variant title:
Welding procedure specification : no. 5:1-2-1
Copyright Claimant:
National Certified Pipe Welding Bureau
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 4:3-2-2 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E8018-B2 without postweld heat treatment
example document: Welding procedure specification number 4:3-2-2 for shielded metal arc welding (S M A W) of chromium molybdenum steel to carbon molybdenum steel using E8018-B2 without postweld heat treatment
Welding procedure specification
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002581494 / 1988-08-24
Date of Publication:
May 4, 1987
Date of Creation:
1987
Title:
Welding procedure specification : no. 5:1-2-2 : for shielded metal arc welding (S M A W) of chromium molybdenum steel pipe, valves, fittings, and flanges to carbon steel pipe, valves, fittings, and flanges using E9018-B3 with postweld heat treatment.
Description:
4 p.
Variant title:
Welding procedure specification : no. 5:1-2-2
Copyright Claimant:
National Certified Pipe Welding Bureau
Names:
National Certified Pipe Welding Bureau
Welding procedure specification
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002581495 / 1988-08-24
Date of Publication:
July 8, 1987
Date of Creation:
1987
Title:
Welding procedure specification : no. 1-47-1 : for gas tungsten arc welding (G T A W) and gas metal arc welding with fluxcore wire (G M A W-F C) manual or semi-automatic of carbon steel pipe, valves, fittings, and flanges with consumable insert with or without postweld heat treatment.
Description:
4 p.
Variant title:
Welding procedure specification : no. 1-47-1
Copyright Claimant:
National Certified Pipe Welding Bureau
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-7-1 for gas metal arc welding using fluxcore wire (G M A W-FC), semi-automatic or machine of carbon steel with and without postweld heat treatment
example document: Welding procedure specification number 1-7-1 for gas metal arc welding using fluxcore wire (G M A W-FC), semi-automatic or machine of carbon steel with and without postweld heat treatment
Welding procedure specification
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002581496 / 1988-08-24
Date of Publication:
July 9, 1987
Date of Creation:
1987
Title:
Welding procedure specification : no. 1-48-1 : for gas tungsten arc welding (G T A W) and submerged arc welding (S A W) manual or machine of carbon steel pipe, valves, fittings, and flanges with consumable insert.
Description:
4 p.
Variant title:
Welding procedure specification : no. 1-48-1
Copyright Claimant:
National Certified Pipe Welding Bureau
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 41-12 for gas tungsten arc welding (G T A W) of nickel pipe, valves, fittings, and flanges
example document: Welding procedure specification number 41-12 for gas tungsten arc welding (G T A W) of nickel pipe, valves, fittings, and flanges
Welding procedure specification (WPS)
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002946549 / 1988-08-24
Date of Publication:
November 5, 1987
Date of Creation:
1987
Title:
Welding procedure specification (WPS) : no. 41-2-1, 41-3-1, 41-32-1 ... [et al.]
Basis of Claim:
New Matter: additions.
Copyright Note:
C.O. correspondence.
Variant title:
Welding procedure specification (WPS) : no. 41-2-1, 41-3-1, 41-32-1 ... [et al.]
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1-37-1 for gas tungsten arc welding (G T A W) and gas metal arc welding (S A W) with fluxcore wire (G M A W-F C), manual of [i.e. or] semi-automatic of carbon steel without consumable insert and without postweld heat treatment
example document: Welding procedure specification number 1-37-1 for gas tungsten arc welding (G T A W) and gas metal arc welding (S A W) with fluxcore wire (G M A W-F C), manual of [i.e. or] semi-automatic of carbon steel without consumable insert and without postweld heat treatment
Welding procedure specification (WPS)
Type of Work:
Non-dramatic literary work
Registration Number / Date:
TX0002946550 / 1988-08-24
Date of Publication:
August 5, 1987
Date of Creation:
1987
Title:
Welding procedure specification (WPS) : no. 8-2-1, 8-3-1, 8-32-1 ... [et al.]
Basis of Claim:
New Matter: additions.
Copyright Note:
C.O. correspondence.
Variant title:
Welding procedure specification (WPS) : no. 8-2-1, 8-3-1, 8-32-1 ... [et al.]
Copyright Claimant:
National Certified Pipe Welding Bureau
Notes:
Cataloged from appl.
Names:
National Certified Pipe Welding Bureau (92 documents)
example document: Welding procedure specification number 1.13 for shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings and flanges using iron power, low hydrogen electrodes with preheat and postweld heat treatment
example document: Welding procedure specification number 1.13 for shielded metal arc welding (S M A W) of carbon steel pipe, valves, fittings and flanges using iron power, low hydrogen electrodes with preheat and postweld heat treatment
This website is not affiliated with document authors or copyright owners. This page is provided for informational purposes only. Unintentional errors are possible. Multiple persons can share the same name.